Two-step heating method delivers flat, highly ordered ultrathin magnetic films (IMAGE)
Caption
The researchers fabricated 5-nm-thick L10-FePd films using a two-step heating process: low-temperature deposition for smooth layer-by-layer growth, followed by 600°C annealing to promote atomic ordering.
Credit
Professor Hiroshi Naganuma from the University of Toyama, Japan
Usage Restrictions
Cannot be reused without permission
License
Original content