Plasma-mediated CL-SRM. (IMAGE)
Caption
(a) Schematic illustration of the CL-SRM process, comprising a POM step and a WS step. (b) Average CH4 conversion during 6 min of CL-SRM under purely thermal and plasma-mediated conditions over LaFeO3 and LaCeFe as a function of bed temperature. The continuous flow rates of CH4/N2 (5/45 cm3∙min−1) and H2O/N2 (5/45 cm3∙min−1) were applied during the 6 min POM and 25 min WS steps, respectively. The mass of the packed oxygen carrier was 1.5 g. The plasma power during the POM step was approximately 25 W. Note: The bed temperature (T) increased by approximately 100 °C when DBD was applied during the plasma-mediated POM step.