(a-b) Characterizations of CuO500/CC after electrolysis: (a) Cu 2p XPS and (b) XRD after electrolysis for 1 h (red), 5 h (blue), and CC (black). (c) NH3 concentration of CuO/CC in the presence or absence of NO3-, CC, and open potential conditions at -0.80 V (vs. RHE). (d) 1H-NMR of 14NH4+ and 15NH4+, (e) Calculated free energy diagram of NO3RR on Cu (111) and Cu(OH)2 (021).