Figure 2 | In situ monitoring of the enhanced surface potential of the MHP film using the KPFM probe as a scraper. (IMAGE)
Caption
Figure 2 | In situ monitoring of the enhanced surface potential of the MHP film using the KPFM probe as a scraper. Surface potential distributions of the MAPbBr3 film (20 μm × 20 μm) with different scanning times within a 10 μm × 10 μm area (marked by green dash lines): (a) pristine, (b) 1 scan, and (c) 10 scans; Top: height diagram and bottom: surface potential mapping, respectively. (d) PL spectra of MAPbBr3 films scanned by 0, 1 and 10 times, respectively, using the KPFM probe. (e) Correlation between changes in the surface charge density and the PL intensity and scan times using the KPFM probe.
Credit
Xin Guo et al.
Usage Restrictions
Credit must be given to the creator.
License
CC BY